Antiques & Collectibles Architectural Ceramics Artists & Potters Artist-in-Residencies Ceramics in the USA Ceramic Societies Ceramics & Women Ceramic Supplies Competitions Commercial Sites Educational Institutions Events Calendar Galleries Glass Arts Glaze Software Health and Safety History & Archaeology Industrial Ceramics Kilns & Firing Magazines Museums Native American Paperclay Porcelain Potteries Raku Repair & Restoration Sculpture Styles Techniques Teapots Technical Info Theory & Criticism Tiles Tuition & Workshops Virtual Ceramics Wedgwood West Coast Funk Woodfiring
Terry Davies Certaldo Florence Italy terrydavies@terrydavies.it http://www.terrydavies.it wood fired bottle 30cm ht. wood fired stoneware, with temoku glaze. I am an English potter working in Tuscany Italy, firing in both wood and gas soda and natural ash glazing. MAIN INDEX | NEW | ROOM 1 | ROOM 2 | ROOM 3 | ROOM 4 | ROOM 5
Terry Davies
Certaldo Florence Italy terrydavies@terrydavies.it http://www.terrydavies.it
wood fired bottle
30cm ht. wood fired stoneware, with temoku glaze.
I am an English potter working in Tuscany Italy, firing in both wood and gas soda and natural ash glazing.