Bloomingdale, IL (USA)
                http://www.milkywayceramics.com
            
            
               
            
            
              
            
            
               
 
            
            
              Untitled (2001)
                
                9 in. diameter
                Thrown and altered cone 6 porcelaneous body. Fired in an electric 
                kiln to
                cone 6, crash cooled to holding temperature for crystal growth 
                to occur. 
                Satin variegated yellow and crystalline glazes on the rim and 
                center, respectively.