Kilns
and Kiln Firing
Technical
Data Part II
Temperature Measurement Color Scale Chart
|
Celsius |
Fahrenheit |
| Lowest visible red |
475° C |
525° F |
| Lowest visible red to dark red |
475-650° C |
525-1202° F |
| Dark red to cherry red |
650-750° C |
1202-1382° F |
| Cherry red to bright cherry red |
750-800° C |
1382-1472° F |
| Bright cherry red to orange |
800-900° C |
1472-1652° F |
| Orange to yellow |
900-1100° C |
1652-2012° F |
| Yellow to light yellow |
1100-1300° C |
2012-2372° F |
| Light yellow to white |
1300-1550° C |
2372-2822° F |
| White to dazzling white |
1550° C and higher |
2822° F and higher |